System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Celcon® M270™ POM, Unfilled
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
Material Notes:
Celcon« acetal copolymer grade M270Ö is a lower molecular weight, high - flow grade designed for superior moldability in multi-cavity, intricate or hard to fill molds applications.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.41
g/cc
1.41
g/cc
ASTM D792
Density
1.41
g/cc
0.0509
lb/in³
ISO 1183
Density of Compound
1.20
g/cc
0.0434
lb/in³
Moisture Absorption
0.200 %
0.200 %
23°C/50%RH; ISO 62
Water Absorption at Saturation
0.75 %
0.75 %
ISO 62
Linear Mold Shrinkage, Flow
0.017
cm/cm
0.017
in/in
ISO 294-4
0.022
cm/cm
0.022
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.016
cm/cm
0.016
in/in
ISO 294-4
0.018
cm/cm
0.018
in/in
ASTM D955
Melt Flow
23
g/10 min
@Load 2.16 kg,
Temperature 190 °C
23
g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
60.7
MPa
8800
psi
ASTM D638
67.0
MPa
9720
psi
50mm/min; ISO 527-2/1A
Elongation at Yield
8.0 %
8.0 %
50mm/min; ISO 527-2/1A
Tensile Modulus
2.80
GPa
406
ksi
50mm/min; ISO 527-2/1A
Flexural Modulus
2.59
GPa
375
ksi
ASTM D790
2.75
GPa
399
ksi
ISO 178
Izod Impact, Notched
0.534
J/cm
1.00
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
5.40
kJ/m²
2.57
ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched
11.6
J/cm²
55.2
ft-lb/in²
ISO 179/1eU
10.8
J/cm²
@Temperature -30.0 °C
51.4
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
0.520
J/cm²
2.47
ft-lb/in²
ISO 179/1eA
Tensile Creep Modulus, 1 hour
2300
MPa
334000
psi
ISO 899-1
Tensile Creep Modulus, 1000 hours
1300
MPa
189000
psi
ISO 899-1
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
110
µm/m-°C
61.1
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
120
µm/m-°C
66.7
µin/in-°F
ISO 11359-2
Specific Heat Capacity
2.21
J/g-°C
0.528
BTU/lb-°F
Thermal Conductivity
0.155
W/m-K
1.08
BTU-in/hr-ft²-°F
Melting Point
166
°C
331
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi)
156
°C
313
°F
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
103
°C
217
°F
ISO 75-1, -2
110
°C
230
°F
ASTM D648
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
-
120
°C
176
-
248
°F
cavity
180
-
200
°C
356
-
392
°F
hot runner
Zone 1
170
-
180
°C
338
-
356
°F
Zone 2
180
-
190
°C
356
-
374
°F
Zone 3
180
-
190
°C
356
-
374
°F
Zone 4
190
-
200
°C
374
-
392
°F
Die Temperature
190
-
200
°C
374
-
392
°F
Melt Temperature
180
-
200
°C
356
-
392
°F
Ejection Temperature
140
°C
284
°F
Drying Temperature
80.0
-
100
°C
176
-
212
°F
Dry Time
3.00
hour
3.00
hour
Injection Pressure
60.0
-
120
MPa
8700
-
17400
psi
Hold Pressure
60.0
-
120
MPa
8700
-
17400
psi
Back Pressure
<=
4.00
MPa
<=
580
psi
Descriptive Properties
Injection molding
Yes
Injection speed
slow-medium
Pellets
Yes
Processing conditions acc. ISO
9988-2
Profile extrusion
No
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celcon® M90™ POM, Unfilled
Celanese Celcon® M270UV POM, UV Resistant
Celanese Zytel® 101 NC010 PA66
420 Stainless Steel
Celanese Celcon® GC25A POM, 25% Glass Reinforced
PHCQ120 / 178575
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.