MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase TPSiV® 4200-50A Thermoplastic Silicone Vulcanizate  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV); Silicone, Thermoplastic

Material Notes: FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistance
APPLICATIONS: Solution for soft touch overmolding on consumer electronics, mobile communication devices, computers, and sport &leisure applications.; Seals and enclosures.

Information provided by Multibase. Multibase is now a DuPont brand; this grade was discontinued prior to DuPont's acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 1183
Linear Mold Shrinkage 0.020 - 0.040 cm/cm0.020 - 0.040 in/in
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 190 °C
10 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5454ISO 868
Tensile Strength 7.00 MPa1020 psiISO 37
Tensile Strength, Ultimate 2.00 MPa290 psiISO 37
Elongation at Break 600 %600 %ISO 37
Flexural Strength 1.19 MPa173 psiISO 178
Flexural Modulus 0.02001 GPa2.902 ksiISO 178
Tear Strength 26.2 kN/m149 pliISO 34
Taber Abrasion, mg/1000 Cycles 8686ASTM D3389
Compression Set  16 %
@Temperature 23.0 °C,
Time 79200 sec
16 %
@Temperature 73.4 °F,
Time 22.0 hour
ISO 815
 65 %
@Temperature 70.0 °C,
Time 79200 sec
65 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Feed Temperature 160 - 170 °C320 - 338 °F
Middle Barrel Temperature 165 - 175 °C329 - 347 °F
Front Barrel Temperature 170 - 180 °C338 - 356 °F
Nozzle Temperature 180 - 200 °C356 - 392 °F
Melt Temperature 190 °C374 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 65.0 - 80.0 °C149 - 176 °F
Dry Time 2 - 4 hour2 - 4 hour
 
Descriptive Properties
Injection SpeedMED-FAST

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 4100-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 4000-70A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 4200-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3111-60A Thermoplastic Silicone Vulcanizate

PMULTI409 / 133559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.