MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chicago Extruded Metals BioBrass® UNS C95510 As-Cast Aluminum Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: This alloy is registered with the U.S. EPA as Antimicrobial.

Information provided by Chicago Extruded Metals

Key Words: AMS 4880, SAE J461, SAE J462
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 9.7 - 10.9 %9.7 - 10.9 %
Copper, Cu >= 78 %>= 78 %
Iron, Fe 2.0 - 3.5 %2.0 - 3.5 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nickel, Ni 4.5 - 5.5 %4.5 - 5.5 %
Other, total 0.20 %0.20 %
Tin, Sn <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.30 %<= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK 230 Cast UNS C95500 Aluminum Bronze
MetalTek MTEK 175-C Cast UNS C95400HT Aluminum Bronze
MetalTek MTEK 175 Cast UNS C95400 Aluminum Bronze
AISI 4140 Steel, oil quenched, 13 mm (0.5 in.) round (845°C (1550°F) quench, 595°C (1100°F) temper)
Chicago Extruded Metals BioBrass® UNS C95520 As-Cast Aluminum Bronze

NCHICA925 / 147644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.