MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovako 100Cr6 803D Steel, Q/T (martensite)
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 5000 Series Steel; Low Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: General Information: 100Cr6 is a through hardening bearing steels intended for rolling contact and other high fatigue applications. In the hardened condition the high hardness, high strength and high cleanliness provides the steel with the right properties to withstand high cycle, high stress fatigue. 100Cr6 is mainly used for small and medium sized bearing components. It is also regularly used for other machine components that require high tensile strength and high hardness. The hardenability approximately corresponds to a ring with max. 17 mm wall thickness. Variant 5620 is offered as 803F or 100Cr6 This steel is delivered in a number of variants. The most common are listed below.

IQ-Steel
803Q - Isotropic properties and better fatigue strength due to higher cleanliness levels, and a finer size and distribution of non-metallic inclusions

BQ-Steel
803Z - Improved cold forming properties due to the reduced silicon content
803D - Improved machinability due to the higher sulphur content.
803P - With a reduced sulphur content to reduce the number of sulphide inclusions
803A - With a reduced controlled sulphur content to reduce the number of sulphide inclusions but ensure consistent machinability
803F - With a controlled sulphur content for consistent machining properties
803N - Slightly increased carbon range to meet the requirements of some international standards
803J – Standard
5620 - A continuous cast variant of 100Cr6

IQ-SteelIQ-Steel® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

BQ-Steel:BQ-steel® is a bearing quality clean steel optimized for fatigue strength and is also ideal for new design solutions outside the bearing industry.

Information provided by Ovako

Key Words: SS 2258, SAE 52100, WNr. 1.3505 , 100 Cr 6 , SUJ2S, SUJ2Z, 100C6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6161
Tensile Strength 2300 MPa334000 psi
Tensile Strength, Yield >= 1700 MPa>= 247000 psi
Elongation at Break 2.0 %2.0 %
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 218 °C424 °FMS
 745 °C1370 °FAC1
 910 °C1670 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.98 - 1.05 %0.98 - 1.05 %
Chromium, Cr 1.4 - 1.6 %1.4 - 1.6 %
Iron, Fe 96.22 - 97.1 %96.22 - 97.1 %As Balance
Manganese, Mn 0.30 - 0.40 %0.30 - 0.40 %
Molybdenum, Mo <= 0.080 %<= 0.080 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Sulfur, S 0.017 - 0.023 %0.017 - 0.023 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 86B50 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, round
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Ovako 100Cr6 803Q Steel, Q/T (martensite)
Ovako 100Cr6 803N Steel, Q/T (martensite)
Ovako 100Cr6 803Z Steel, Q/T (martensite)

NOVAKO010 / 234309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.