MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good stiffness even at higher temperatures.

Xmod GD301HP has been developed especially for the fluid engineering and automotive market for applications which require high mechanical strengths at high service temperatures. These include pump housings, valves, pedal carriers, and technical components under the bonnet.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow <= 0.0020 cm/cm
@Thickness 2.00 mm
<= 0.0020 in/in
@Thickness 0.0787 in
In Flow Direction; Borealis Method
Linear Mold Shrinkage, Transverse >= 0.010 cm/cm>= 0.010 in/inBorealis Method
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Spiral Flow 95.0 cm
@Thickness 2.00 mm,
Temperature 250 °C
37.4 in
@Thickness 0.0787 in,
Temperature 482 °F
Borealis Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 45.0 MPa
@Temperature 100 °C
6530 psi
@Temperature 212 °F
ISO 527-2
Tensile Strength, Yield 108 MPa15700 psiAt 50 mm/min; ISO 527-2
Elongation at Break 2.9 %2.9 %ISO 527-2
 7.5 %
@Temperature 100 °C
7.5 %
@Temperature 212 °F
ISO 527-2
Tensile Modulus 8.10 GPa1170 ksiISO 527-2
 3.50 GPa
@Temperature 100 °C
508 ksi
@Temperature 212 °F
ISO 527-2
Flexural Strength 145 MPa21000 psiISO 178
Flexural Modulus 6.80 GPa986 ksiISO 178
Flexural Strain at Yield 3.2 %3.2 %ISO 178
Charpy Impact Unnotched 4.70 J/cm²22.4 ft-lb/in²ISO 179/1eU
 4.40 J/cm²
@Temperature -20.0 °C
20.9 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 0.950 J/cm²4.52 ft-lb/in²ISO 179/1eA
 0.850 J/cm²
@Temperature -20.0 °C
4.05 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
Impact Test 5.00 J
@Temperature -20.0 °C
3.69 ft-lb
@Temperature -4.00 °F
ISO 6603T
 6.50 J
@Thickness 3.00 mm
4.79 ft-lb
@Thickness 0.118 in
Biaxial, Total Energy; ISO 6603T
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FHDT-A; ISO 75-2
Vicat Softening Point 138 °C280 °FB (50 N); ISO 306
Shrinkage <= 1.55 %<= 1.55 %Testbox; Borealis Method
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 270 °C428 - 518 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PP-GF25-0403 P10/10 PP, 25% Glass Reinforced
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene
A. Schulman Diamond NPP25-1503 GF30 30% Glass Filled Copolymer Polypropylene
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
LG Chemical LUPOL GP2300 PP+GF30%

PBOREA210 / 27517

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.