MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2700 S-30A MD NATURAL Saturated Styrenic Block Copolymer ISO 10993 Tested
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: ISO 10993 is used to evaluate the biocompatibility of medical devices. Consult RTP Company for more details.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D 792
Linear Mold Shrinkage 0.020 - 0.030 cm/cm
@Thickness 3.20 mm
0.020 - 0.030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30
@Time 10.0 sec
30
@Time 0.00278 hour
ASTM D 2240
Tensile Strength at Break 5.17 MPa
@Thickness 3.20 mm
750 psi
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Elongation at Break 700 %
@Thickness 3.20 mm
700 %
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 20.2 kN/m115 pliDie C; ASTM D 624
Compression Set  10 %
@Temperature 23.0 °C,
Time 79200 sec
10 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B, Type 2; ASTM D 395
 37 %
@Temperature 70.0 °C,
Time 79200 sec
37 %
@Temperature 158 °F,
Time 22.0 hour
Method B, Type 2; ASTM D 395
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 - 204 °C350 - 400 °F
Mold Temperature 15.6 - 37.8 °C60.0 - 100 °F
Drying Temperature 76.7 °C
@Time 7200 sec
170 °F
@Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2720 S-30A Saturated Styrenic Block Copolymer
Avient Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE)
Teknor Apex Medalist® MD-110 Thermoplastic Elastomer
Teknor Apex Medalist® MD-115 Thermoplastic Elastomer

PQZVA17323 / 120543

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.