MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Flint Hills PP 23R2A Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliant

Features: High contact clarity, non-blushing, toughness, impact, chemical, solvent, stress crack resistance, stiffness, hardness, heat resistance, exceptional high clarity and impact strength.

Applications: Blow molded: radiation sterilizable vials and bottles.

FDA Notes: 21 CFR 177.1520 (c)3.2; under conditions of use B through H described in 21 CFR 176.170 Table 2

Former Huntsman polypropylene products are now produced by Flint Hills Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Break >= 700 %>= 700 %ASTM D638
Modulus of Elasticity 1.015 GPa147.2 ksiASTM D638
Flexural Modulus 0.940 GPa136 ksiASTM D790
Izod Impact 80.0 J59.0 ft-lbNotched; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills PP 13R9A Random Copolymer Polypropylene
Flint Hills PP 13T10A cs279 Random Copolymer Polypropylene
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Braskem H521 Homopolymer Polypropylene
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin

PHUN88 / 47697

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.