MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake EM811AA Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.

    Application/Uses
  • Flexible medical
  • Medical

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: High flow and low stiffness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³ASTM D1505
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 9.00 MPa1310 psi500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 300 %300 %500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 0.200 GPa29.0 ksi12.7mm/min; ASTM D790
 
Processing PropertiesMetricEnglishComments
Melt Temperature 149 - 166 °C300 - 330 °F
 
Descriptive Properties
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake EM182AA Low Density Polyethylene
Westlake EM184AA Low Density Polyethylene
Westlake EC811AA Low Density Polyethylene
LyondellBasell Montell 1900 UHMW Polyethylene
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch

PWESF089 / 84526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.