Forms: Pellets
Filler/Reinforcement: Glass Fiber Reinforcement, 33% Filler by Weight
Additive: Heat Stabilizer and Lubricant
Features: Flame Retardant, Heat Stabilized and Lubricated
TPCI# 656102