MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: Key Feature: Flame retardant V-0 UL-94 class

Applications: Ultra-precise components

General features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemical & weather resistance, and processability.

Information provided by Toyobo Co., Ltd

Key Words: Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ASTM D792
Water Absorption 0.050 %0.050 %ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength, Ultimate 172 MPa24900 psiASTM D638
Elongation at Break 1.9 %1.9 %ASTM D638
Flexural Yield Strength 255 MPa37000 psiASTM D790
Flexural Modulus 16.0 GPa2320 ksiASTM D790
Compressive Yield Strength 128 MPa18600 psiASTM D695
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
Taber Abrasion, mg/1000 Cycles 3434ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance 80 sec80 secASTM D495
Comparative Tracking Index 200 V200 VIEC test
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FASTM D648
UL RTI, Electrical 130 °C266 °FUL-746B
Flammability, UL94 V-0
@Thickness 0.7937 mm
V-0
@Thickness 0.03125 in
unregistered

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant
Toyobo Vylopet® EMC130-04 Glass Reinforced Polyester, Easy Molding Grade
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade

PTOY33 / 70705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.