MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Fibre Glast 180 Clear Gel Coat
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: #180 Clear Gel Coat is a high performance, premium quality gel coat for both airless and air atomized spray applications. #180 offers UV light stability, excellent clarity, crack and chemical resistance. This deep, crystal-clear and non-yellowing gel coat is compatible with underwater and water contact marine applications as well as sanitary ware such as showers and tubs. It is recommended to be used as a protective clear coat over Chromaveil™, other colors or glitterflake. Blend with #1040 Duratec Hi-Gloss Additive when top coating. Requires 1.5% MEKP

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  10000 - 13000 cP
@Shear Rate 0.1 1/s,
Temperature 25.0 °C
10000 - 13000 cP
@Shear Rate 0.1 1/s,
Temperature 77.0 °F
LVF#4, Uncured
 17000 - 22000 cP
@Shear Rate 1 1/s,
Temperature 25.0 °C
17000 - 22000 cP
@Shear Rate 1 1/s,
Temperature 77.0 °F
LVF#4, Uncured
Viscosity Measurement 5.9 - 6.55.9 - 6.5Thix Index, Uncured
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Gel Time 8.00 - 10.0 min8.00 - 10.0 min
 
Descriptive Properties
Peak Cure Exotherm390-405°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Q-Cel® 5028
SPHERE ONE EXTENDOSPHERES™ XOL-150 Hollow Spheres
Potters Industries Q-Cel® 5023
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres
Saxonburg Ceramics S-213 Cordierite

PFIBRE102 / 104539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.