MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough materials, highly resistant to contamination, and will not be affected by other chemicals during cure or after. Typical uses: Electronic assemblies and components.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³
Viscosity 16000 cP
@Temperature 25.0 °C
16000 cP
@Temperature 77.0 °F
Linear Mold Shrinkage 0.013 cm/cm0.013 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4242
Tensile Strength, Ultimate 2.65 MPa384 psi
Elongation at Break 170 %170 %
Tear Strength 3.80 kN/m21.7 pliDie B
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 3.6
@Frequency 1000 Hz
3.6
@Frequency 1000 Hz
Dielectric Strength 20.5 kV/mm
@Thickness 1.90 mm
521 kV/in
@Thickness 0.0748 in
Dissipation Factor 0.0050
@Frequency 1000 Hz
0.0050
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 220 µm/m-°C
@Temperature 20.0 °C
122 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °FContinuous useful temperature.
Minimum Service Temperature, Air -115 °C-175 °FContinuous useful temperature.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCure time 24 hrs.
Pot Life 90.0 min
@Temperature 25.0 °C
90.0 min
@Temperature 77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy Adhesive, Flexible
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound

PZZGE979 / 40533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.