MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering S50D Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Black Silicone Rubber, 46-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated to meet UK Ministry of Defence Aircraft Materials Specification DTD5531A Grade 50. ASTM & ISO designation = VMQ.

Applications: Sheets, mouldings and extrusions for mainly mechanical applications in contact with air within the quoted temperature range. They are not intended for liquid sealing or for application where low compression set is of prime importance. Occasional contamination by silicate ester and phosphate ester hydraulic fluids and greases is not unduly detrimental, provided the temperature is not excessive. Contact with fuels, light mineral oils, silicone liquids or greases derived from these should be avoided. Excellent ozone resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050°IRHD; ASTM D1415
 47 - 5747 - 57°IRHD, -3/+7 change after 336 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 5.60 MPa812 psi-20% change after 336 hours @ 200°C; ASTM D412
 7.00 MPa1020 psiASTM D412
Elongation at Break 245 %245 %-30% change after 336 hours @ 200°C; ASTM D412
 350 %350 %ASTM D412
Compression Set 15 %
@Temperature 175 °C,
Time 86400 sec
15 %
@Temperature 347 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 -65.0 °C-85.0 °FNon-brittle after 3 minutes
Flash Point >= 300 °C>= 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering S60X Silicone Rubber
Precision Polymer Engineering S50N Silicone Rubber
Freudenberg S310 Silicone Elastomer (VMQ)
Precision Polymer Engineering S50A Silicone Rubber
Precision Polymer Engineering S60A Silicone Rubber

PPRECI231 / 57955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.