MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior EcoPaXX® Q-KGS6 PA410-GF30 FR
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: 30% Glass Reinforced, Flame Retardant (Halogen free)

EcoPaXX® is a former DSM Engineering Plastics product line now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³dry; ISO 1183
Moisture Absorption 1.10 %1.10 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0133 cm/cm0.0133 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 90.0 MPa13100 psicond; ISO 527-1/-2
 135 MPa19600 psidry; ISO 527-1/-2
Elongation at Break 2.5 %2.5 %dry; ISO 527-1/-2
 3.8 %3.8 %cond; ISO 527-1/-2
Tensile Modulus 7.70 GPa1120 ksicond; ISO 527-1/-2
 10.0 GPa1450 ksidry; ISO 527-1/-2
Charpy Impact Unnotched  4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eA
 0.750 J/cm²
@Temperature 23.0 °C
3.57 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmcond; IEC 60093
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmdry; IEC 60093
Surface Resistance 6.00e+13 ohm6.00e+13 ohmcond; IEC 60093
Dielectric Strength 30.0 kV/mm762 kV/incond; IEC 60243-1
 40.0 kV/mm1020 kV/indry; IEC 60243-1
Comparative Tracking Index 600 V600 Vcond; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°Fdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 66.0 µm/m-°C36.7 µin/in-°Fdry; ISO 11359-1/-2
Melting Point 250 °C482 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °Fdry; ISO 75-1/-2
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
dry; IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
dry; IEC 60695-11-10
Glow Wire Ignition Temperature 775 °C
@Thickness 0.800 mm
1430 °F
@Thickness 0.0315 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 
Descriptive Properties
Calculated Bio Based Carbon Content (%)60ASTM 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
Envalior Akulon® Ultraflow K-FKGS6/B PA6-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Arnite® TV4 640 (PBT+PC) - GF20
Envalior Arnite® AV2 390 XT PET GF50
Envalior Arnite® AV2 370 XT PET-GF35

PDSM9825 / 161446

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.