MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnFlex™ HT 40A-3S2131 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at elevated temperatures and a high heat resistance. Furthermore, OnFlex™ HT compounds are in compliance with EN 681-2 and offer excellent mechanical properties, a wide hardness range and good processability.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050IRHD; ISO 48
 40
@Temperature 23.0 °C
40
@Temperature 73.4 °F
Injection Molded; DIN 53505
Tensile Strength at Break  4.50 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
653 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
200 mm/min Flow; DIN 53504
 7.80 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
1130 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
200 mm/min Across Flow; DIN 53504
Elongation at Break  620 %
@Thickness 2.00 mm,
Temperature 23.0 °C
620 %
@Thickness 0.0787 in,
Temperature 73.4 °F
200 mm/min Flow; DIN 53504
 790 %
@Thickness 2.00 mm,
Temperature 23.0 °C
790 %
@Thickness 0.0787 in,
Temperature 73.4 °F
200 mm/min Across Flow; DIN 53504
Compression Set  12 %
@Temperature 23.0 °C,
Time 259000 sec
12 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 28 %
@Temperature 70.0 °C,
Time 79200 sec
28 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 45 %
@Temperature 100 °C,
Time 79200 sec
45 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 45 %
@Temperature -10.0 °C,
Time 79200 sec
45 %
@Temperature 14.0 °F,
Time 22.0 hour
ISO 815
 46 %
@Temperature 125 °C,
Time 79200 sec
46 %
@Temperature 257 °F,
Time 22.0 hour
ISO 815
 52 %
@Temperature -10.0 °C,
Time 259000 sec
52 %
@Temperature 14.0 °F,
Time 72.0 hour
ISO 815
 70 %
@Temperature 150 °C,
Time 79200 sec
70 %
@Temperature 302 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °F
 
Descriptive Properties
Change in Shore Hardness in Air-1 Shore ADIN 53505; Shore A, 70°C, 168 hr
Change in Tensile Strain at Break in Air-4%DIN 53504; 70°C, 168 hr, 2.00 mm
Change in Tensile Strength in Air-9%DIN 53504; 70°C, 168 hr, 2.00 mm
Change in Volume0.06%ISO 1817; 70°C, 168 hr, in Water
 20%ISO 1817; 70°C, 72 hr, in ASTM #1 Oil
FeaturesHigh Heat Resistance
 Low Compression Set
 Ozone Resistant
FormsPellets
Generic MaterialTPE
Generic Material TypeStyrenic Thermoplastic Elastomer (TES)
Generic NameThermoplastic Elastomer (TPE)
Injection RateFast
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
Stress Relaxation15%ISO 3384; 23°C; 168hrs, 25% compression, Method A
 28%ISO 3384; 23°C; 100d, 25% compression, Method A
UsesPipe Seals

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Avient OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE)
Avient OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE)
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
Avient OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE)

PH0POL1039 / 145608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.