MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and cement and steel-mill equipment. Resistant to the effects of seizing or galling, low coefficient of friction alloys sliding contact with other metals. Used in equipment where no lubricants are used. Outstanding resistance to cavitation-erosion. Combines wear and corrosion resistance with good impact strength and resistance to thermal shock. Retains high hardness, even at red heat. Electrical conductivity 1.90% compared to Copper. 2360 MPa average modulus of rupture of sheet at room temperature. Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.387 g/cc0.3030 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  102
@Temperature 871 °C
102
@Temperature 1600 °F
Mutual indentation method
 167
@Temperature 760 °C
167
@Temperature 1400 °F
Mutual indentation method
 203
@Temperature 649 °C
203
@Temperature 1200 °F
Mutual indentation method
 226
@Temperature 538 °C
226
@Temperature 1000 °F
Mutual indentation method
Hardness, Knoop 363363
Hardness, Rockwell A 6868Converted from Rockwell C hardness.
Hardness, Rockwell C 3636
Hardness, Vickers 349349
Tensile Strength, Ultimate 1000 MPa145000 psi
Tensile Strength, Yield 621 MPa
@Strain 0.2 %
90100 psi
@Strain 0.2 %
Elongation at Break 12 %12 %in 50.8 mm
Modulus of Elasticity 214 GPa31000 ksisheet at RT
 210 GPa
@Diameter 15.9 mm,
Temperature 23.0 °C
30500 ksi
@Diameter 0.626 in,
Temperature 73.4 °F
bar
Izod Impact Unnotched 84.0 J
@Thickness 12.7 mm
62.0 ft-lb
@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Charpy Impact  8.00 J
@Temperature 23.0 °C
5.90 ft-lb
@Temperature 73.4 °F
Longitudinal
 20.0 J
@Temperature 538 - 816 °C
14.8 ft-lb
@Temperature 1000 - 1500 °F
Longitudinal
Charpy Impact, Unnotched 88.0 J64.9 ft-lbTransverse
 98.0 J
@Temperature 22.2 °C
72.3 ft-lb
@Temperature 72.0 °F
Longitudinal
 110 J
@Temperature 538 °C
81.1 ft-lb
@Temperature 1000 °F
Longitudinal
 157 J
@Temperature 677 °C
116 ft-lb
@Temperature 1250 °F
Longitudinal
 171 J
@Temperature 816 °C
126 ft-lb
@Temperature 1500 °F
Longitudinal
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000910 ohm-cm
@Temperature 22.0 °C
0.0000910 ohm-cm
@Temperature 71.6 °F
Magnetic Permeability <= 1.2
@Temperature 22.0 °C
<= 1.2
@Temperature 71.6 °F
200 Oersted (15.900 A/m)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.9 µm/m-°C
@Temperature 0.000 - 100 °C
7.72 µin/in-°F
@Temperature 32.0 - 212 °F
 14.1 µm/m-°C
@Temperature 0.000 - 200 °C
7.83 µin/in-°F
@Temperature 32.0 - 392 °F
 14.5 µm/m-°C
@Temperature 0.000 - 300 °C
8.06 µin/in-°F
@Temperature 32.0 - 572 °F
 14.7 µm/m-°C
@Temperature 0.000 - 400 °C
8.17 µin/in-°F
@Temperature 32.0 - 752 °F
 15.0 µm/m-°C
@Temperature 0.000 - 500 °C
8.33 µin/in-°F
@Temperature 32.0 - 932 °F
 15.3 µm/m-°C
@Temperature 0.000 - 600 °C
8.50 µin/in-°F
@Temperature 32.0 - 1110 °F
 15.8 µm/m-°C
@Temperature 0.000 - 700 °C
8.78 µin/in-°F
@Temperature 32.0 - 1290 °F
 16.3 µm/m-°C
@Temperature 0.000 - 800 °C
9.06 µin/in-°F
@Temperature 32.0 - 1470 °F
 16.9 µm/m-°C
@Temperature 0.000 - 900 °C
9.39 µin/in-°F
@Temperature 32.0 - 1650 °F
 17.4 µm/m-°C
@Temperature 0.000 - 1000 °C
9.67 µin/in-°F
@Temperature 32.0 - 1830 °F
Specific Heat Capacity 0.423 J/g-°C0.101 BTU/lb-°Fat RT (calculated)
Thermal Conductivity 14.85 W/m-K103.1 BTU-in/hr-ft²-°F
Melting Point 1265 - 1354 °C2309 - 2469 °F
Solidus 1265 °C2309 °F
Liquidus 1354 °C2469 °F
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.57 - 0.700.57 - 0.70reflecting power
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.90 - 1.4 %0.90 - 1.4 %
Chromium, Cr 28 - 32 %28 - 32 %
Cobalt, Co 50 - 67 %50 - 67 %As remainder
Iron, Fe <= 3.0 %<= 3.0 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 1.5 %<= 1.5 %
Nickel, Ni <= 3.0 %<= 3.0 %
Silicon, Si <= 2.0 %<= 2.0 %
Tungsten, W 3.5 - 5.5 %3.5 - 5.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.7 mm thick sheet
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C

NST6BA / 19210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.