MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require:
  • Wide process windows and good flow
  • Long-term UV stabilization
  • Excellent impact strength
  • Excellent ESCR
These resins are available in:
  • Pellet form - HMN TR-938
  • 35 US mesh powder - HMN TR-938G

Applications:

  • Industrial waste containers and tanks
  • Marine equipment

Information provided by Phillips

These resins meet the following specifications:

  • ASTM D4976 - PE 223
  • FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c) Table 2. Single use articles contacting food types I, II, IV-B, VI-A, VI-B, VII-B, and VIII. Repeated use articles contacting all food types defined in 21 CFR 176.170(c) Table 1.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ASTM D-1505
ESCR 100% Igepal® >= 1000 hour>= 1000 hourCondition A, F50; ASTM D-1693
ESCR 10% Igepal® 200 hour200 hourCondition A, F50; ASTM D-1693
Melt Index of Compound 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D-2240
Tensile Strength, Yield 17.0 MPa2470 psi2 in/min, Type IV bar; ASTM D-638
Elongation at Break 700 %700 %2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 0.820 GPa119 ksiTangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
 0.660 GPa
@Strain 2 %
95.7 ksi
@Strain 2 %
Secant; 16:1 span:depth, 0.5 in/min; ASTM D-790
Impact Test  95.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
70.1 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM Impact
 237 J
@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
ARM Impact
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °FASTM D-3418
Crystallization Temperature 113 °C235 °FASTM D-3418
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C144 °FMethod A; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C108 °FMethod A; ASTM D-648
Vicat Softening Point 117 °C243 °FLoading 1, Rate A; ASTM D-1525
Brittleness Temperature -75.0 °C-103 °FType A, Type I specimen; ASTM D-746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals NOVAPOL® TR-0338-UI LLDPE Rotational Molding Resin
ExxonMobil LL 8460 Rotational Molding Resin
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE
Celanese Ateva® 1821A Film Ethylene Vinyl Acetate Copolymer Film
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin

PCHEVD234 / 20728

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.