MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Asahi Kasei Leona™ 9400S Polyamide 66, High Molecular Weight
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Excellent impact resistance. Suitable for thick-wall parts.

Applications:Railroad tie insulators

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccDry as Molded; ASTM D792
Moisture Absorption at Equilibrium 2.8 %
@Temperature 23.0 °C
2.8 %
@Temperature 73.4 °F
50% RH
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575Dry as Molded; ASTM D785
Tensile Strength 44.0 MPa6380 psiConditioned at 50% RH; ASTM D638
 79.0 MPa11500 psiDry as Molded; ASTM D638
Elongation at Break 60 %60 %Dry as Molded; ASTM D638
 260 %260 %Conditioned at 50% RH; ASTM D638
Flexural Strength 44.0 MPa6380 psiConditioned at 50% RH
 108 MPa15700 psiDry as Molded
Flexural Modulus 0.800 GPa116 ksiConditioned at 50% RH; ASTM D790
 2.60 GPa377 ksiDry as Molded; ASTM D790
Izod Impact, Notched 0.540 J/cm1.01 ft-lb/inDry as Molded; ASTM D256
 2.74 J/cm5.13 ft-lb/inConditioned at 50% RH; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDry as Molded; ASTM D257
Dielectric Strength 20.0 kV/mm508 kV/inDry as Molded; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FDry as Molded; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® FP-EF-103 PTFE, 15% Glass Filled
Avient Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated

PASAHI8126 / 221153

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.