MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Premix Thermoplastics PRE-ELEC® 12-000
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has an excellent balance of mechanical properties with good impact strength. PRE-ELEC 12-000 is easy to extrude or injection mold.

Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
Linear Mold Shrinkage 0.020 - 0.025 cm/cm0.020 - 0.025 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
Elongation at Break 6.0 %6.0 %ISO 527
Tensile Modulus 3.40 GPa493 ksiISO 527
Izod Impact, Notched 0.690 J/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
1.29 ft-lb/in
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched 7.40 J/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
13.9 ft-lb/in
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmISO D-257
Surface Resistance <= 1e+05<= 1e+05ISO D-257
Static Decay <= 2.0 sec<= 2.0 secISO IEC 61340-5-1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FISO 75/Method Af
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 210 °C365 - 410 °F
Mold Temperature 80.0 - 105 °C176 - 221 °F
Drying Temperature 80.0 °C
@Time 10800 - 14400 sec
176 °F
@Time 3.00 - 4.00 hour
Pre-drying in a dehumidifier
Injection Pressure 60.0 - 80.0 MPa8700 - 11600 psi
 
Descriptive Properties
Injection SpeedModerate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound
Avient Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound
Röchling SUSTARIN® H AF - DE588 POM/Acetal Homopolymer
DuPont Mobility and Materials Delrin® FG570 NC000 Acetal Homopolymer

PPREMA000 / 58013

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.