MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Celcon® LW270AS Low Wear and Anti-Static Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Celcon LW270AS is a M270-based product which provides both low wear and anti-static properties.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %at 50% RH; ISO 62
Water Absorption at Saturation 0.65 %0.65 %ISO 62
Melt Flow 25.8 g/10 min25.8 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 53.0 MPa7690 psi50 mm/min; ISO 527-2/1A
Flexural Modulus 2.31 GPa335 ksiISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °F
Mold Temperature 77.0 - 93.0 °C171 - 199 °F
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Injection Pressure 75.8 - 110 MPa11000 - 16000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 13021 RM Acetal Copolymer
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin
Celanese Celcon® UV270Z - CST Lubricated and Stabilized Acetal Copolymer
Celanese Celcon® TX90PLUS Acetal Copolymer
Celanese Celcon® MT8U01 Medical Grade Acetal Copolymer

PHCW12 / 45953

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.