MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Avient Edgetek® SF-10GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes:

Description/Features:

  • Glass Fiber Reinforced
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.406 g/cc1.406 g/ccASTM D792
Water Absorption 0.050 %0.050 %24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0055 cm/cm0.0050 - 0.0055 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 68.9 MPa10000 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 4.0 %4.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 5.52 GPa800 ksiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 5.52 GPa800 ksiASTM D790
Izod Impact, Notched 0.641 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C350 °FAnnealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FAnnealed, 0.125 in bars; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 316 °C550 - 600 °FMolding
Mold Temperature >= 135 °C>= 275 °F
Drying Temperature 135 °C275 °F
Dry Time 2 hour2 hour
 
Descriptive Properties
Product FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Avient OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS)
Avient Edgetek® SF-30GF/000 Polyphenylene Sulfide (PPS), Glass Filled
Avient Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL

PH1PO0780 / 43719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.