MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram PlusTek RA331G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% Glass-fiber reinforced Nylon 66 for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 160 MPa23200 psiISO 527
Elongation at Break 2.3 %2.3 %ISO 527
Flexural Strength 220 MPa31900 psiISO 178
Flexural Modulus 7.80 GPa1130 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 90.0 kV/mm2290 kV/inIEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 259 °C498 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek RA334G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek RA325G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced, Flame Retardant, Halogen Free
Polyram PlusTek RA321G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant
Polyram PlusTek RA300G6 Nylon 6.6, 30% Glass Fiber

PPOLYR863 / 126662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.