MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Sumitomo Bakelite RX® 2-501N Diallyl Phthalate Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP), Cast, Mineral Filler

Material Notes: RX® 2-501N is a mineral filled ISO diallyl phthalate compound which conforms with the requirements of ASTM D5948 Type MIG.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccASTM D792
Apparent Bulk Density 0.750 g/cc0.0271 lb/in³ASTM D1895
Water Absorption 0.30 %
@Time 173000 sec
0.30 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.0 MPa7980 psiASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 11.7 GPa1700 ksiASTM D790
Compressive Strength 145 MPa21000 psiASTM D695
Izod Impact, Notched 0.240 J/cm0.450 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
wet; ASTM D150
Dissipation Factor 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 150 sec150 secASTM D495
Track Resistance >= 600 sec>= 600 secASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FASTM E831
Thermal Conductivity 23.0 W/m-K160 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 130 °C266 °FUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 274 °C525 °FAs Molded; ASTM D648A
Flammability, UL94  HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cosmic Plastics FARBOSET® 5000 Black Mineral and Glass Filled Epoxy Molding Compound
Atom Adhesives AA-DUCT AD1 Silver Filled Epoxy Adhesive
Envalior Stanyl® TC153 PA46 FR(17)
IIMAK METALLOGRAPH™ Conductive Thermal Transfer Ribbon
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced

PSUMIT740 / 194545

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.