MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec MZ 429 Zirconia, ZrO2-Y2O3
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: MZ 429 is a yttria-stabilized zirconia ceramic.

Key Words: Zirconium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.05 g/cc0.219 lb/in³DIN EN 623-2
Water Absorption 0.00 %0.00 %Open Porosity; DIN EN 623-2
Permeability 0.000.00%, Gas
Weibull Modulus >= 10>= 10DINV ENV 843-5
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 12501250HV1; DINV ENV 843-4
Tensile Modulus 210 GPa30500 ksiYoung's; DINV ENV 843-2
Flexural Strength 1050 MPa152000 psiDIN EN 843-1
Compressive Strength 2200 MPa319000 psiDIN 51067T1
Poissons Ratio 0.300.30DINV ENV 843-2
Fracture Toughness 6.50 MPa-m½5.92 ksi-in½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 80.8 GPa11700 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 672-1
Dielectric Constant 29
@Frequency 1e+6 Hz
29
@Frequency 1e+6 Hz
IEC 672-1
Dielectric Strength 17.0 kV/mm432 kV/inIEC 672-1
Dielectric Loss Index 0.0020
@Frequency 1e+9 Hz
0.0020
@Frequency 1e+9 Hz
IEC 672-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.17 µin/in-°F
@Temperature 68.0 - 212 °F
DIN EN 821-1
 11.2 µm/m-°C
@Temperature 20.0 - 400 °C
6.22 µin/in-°F
@Temperature 68.0 - 752 °F
DIN EN 821-1
 11.6 µm/m-°C
@Temperature 20.0 - 600 °C
6.44 µin/in-°F
@Temperature 68.0 - 1110 °F
DIN EN 821-1
 11.7 µm/m-°C
@Temperature 20.0 - 1000 °C
6.50 µin/in-°F
@Temperature 68.0 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°FDINV ENV 821-3
Thermal Conductivity 2.50 W/m-K17.4 BTU-in/hr-ft²-°FDIN EN 821-2
Maximum Service Temperature, Air 1000 °C1830 °F
Maximum Service Temperature, Inert 1000 °C1830 °F
 
Descriptive Properties
Ra = Arithmetic Mean Roughness Value (µm)<0.06
Thermal Shock Resistance R1 (K)321calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec 848 Zirconia, ZrO2•MgO
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
CeramTec ZN 40 Zirconia, ZrO2-MgO
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2

CCERA912 / 107512

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.