MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis HB601WG Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical properties and is easy to process. Applications: HB601WG has been developed especially for applications like household applications, dishwasher components, and washing machine parts.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inaverage process; 150x80x2mm
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inaverage process; 150x80x2mm
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.2 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 65.0 MPa9430 psi358 N/30s; ISO 2039
Tensile Strength, Yield 34.0 MPa4930 psiISO 527-2
Elongation at Yield 10 %10 %50mm/min; ISO 527-2
Tensile Modulus 1.40 GPa203 ksi1mm/min; ISO 527-2
Flexural Strength 40.0 MPa5800 psiISO 178
Flexural Modulus 1.40 GPa203 ksi5mm/min; ISO 178
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -20.0 °C
9.52 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C126 °FISO 75-2
Vicat Softening Point  90.0 °C
@Load 5.10 kg
194 °F
@Load 11.2 lb
ISO 306
 154 °C
@Load 1.02 kg
309 °F
@Load 2.25 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
Melt Temperature 220 - 260 °C428 - 500 °Fmass temperature
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Velocity 100 - 200 mm/sec3.94 - 7.87 in/sec
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Back Pressurelow to medium
Screw Speedlow to medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis RB307MO Polypropylene Random Copolymer
Borealis HB600TF Polypropylene
Braskem H 510 Bioriented Film Polypropylene
Covestro Bayblend® T65 XF Polycarbonate + ABS
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature

PBOREA467 / 108726

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.