Market Segment: Consumer Products, Film Suggested Uses Include Housewares, Patio Furniture, Closures Information provided by Sunoco Chemicals. Available in Canada. Braskem acquired Sunoco Chemicals polypropylene product line in 2010. |
Multi Purpose, Good Color and Process Stability |