MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

APCM DA 2406 Two Part Epoxy Adhesive Fast Set
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DA 2406 is a two part, epoxy adhesive which bonds well to wood, metal, fiberglass, and plastics. This adhesive can be mixed in a 1:1 volume ratio and cured at room temperature. Care must be taken when mixing this material, mix the material once for 90 seconds and do not mix it again, use immediately this material sets in 4 to 5 minutes

Information provided by Adhesive Prepegs for Composite Manufacturers, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 33.8 MPa
@Temperature 23.9 °C
4900 psi
@Temperature 75.0 °F
Lap, Cure 24 hrs @75°F
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Pressure 0.0689 MPa,
Temperature 23.9 °C
0.250 hour
@Pressure 10.0 psi,
Temperature 75.0 °F
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
 
Descriptive Properties
ColorTranslucent whitePart A
 Translucent whitePart B
Mix ratio1 part A
 1 part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SIDPEC EGYPTENE® LL 2406 AA LLDPE Pipe Grade
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer

PAPCM016 / 187029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.