MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Envalior Stanyl® TC154 PA46 FR(17)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: Thermal conductive material, Flame Retardant, Heat Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³dry; ISO 1183
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inSim. To ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.0 MPa7980 psidry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %dry; ISO 527-1/-2
Tensile Modulus 5.10 GPa740 ksidry; ISO 527-1/-2
Izod Impact Resistance 0.200 J/cm²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 180/1A
Charpy Impact, Notched 0.200 J/cm²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmdry; IEC 60093
Dielectric Strength 30.0 kV/mm762 kV/indry; IEC 60243-1
Comparative Tracking Index 225 V225 Vdry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 48.0 µm/m-°C26.7 µin/in-°Fdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 48.0 µm/m-°C26.7 µin/in-°Fdry; ISO 11359-1/-2
Thermal Conductivity 0.500 W/m-K3.47 BTU-in/hr-ft²-°Fthrough plane; ASTM E1461
 1.00 W/m-K6.94 BTU-in/hr-ft²-°Fin plane; ASTM E1461
UL RTI, Electrical 140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
dry; IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TC153 PA46 FR(17)
Envalior Stanyl® TC154 PA46 FR(17), Dry, Flame Retardant, Heat Stabilized
Envalior Stanyl® TC551 PA46 FR(17)
Envalior Stanyl® TC153 PA46 FR(17), Dry, Flame Retardant, Heat Stabilized
Envalior Stanyl® TC155 PA46 FR(17)

PDSM9921 / 161542

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.