MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® VTR-9217 Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • high quality, smooth extrudate surface and appearance at thickness below .040” or 1.0 mm
  • excellent ‘green’ strength that helps maintain extrudate shape as well as enables draw down to a thickness of .008” or 0.2 mm.
  • lower viscosity, lower hardness, and better compression set than VTR-9209, the first generation precompound based on the same gum polymer
  • good fuel permeation resistance for a ‘B’ type FKM
  • compounds show good adhesion and physical properties

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/ccUncompounded Viton
Mooney Viscosity 20
@Temperature 121 °C
20
@Temperature 250 °F
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666ASTM D2240
Tensile Strength at Break 7.90 MPa1150 psiASTM D412
Tensile Stress at Strain 0.800 MPa
@Strain 10 %
116 psi
@Strain 10 %
No Postcure; ASTM D412
Elongation at Break 302 %302 %ASTM D412
100% Modulus 3.20 MPa
@Strain 100 %
464 psi
@Strain 100 %
No Postcure; ASTM D412
Compression Set  24 %
@Temperature 70.0 °C,
Time 252000 sec
24 %
@Temperature 158 °F,
Time 70.0 hour
Plied; ASTM D395B
 69 %
@Temperature 150 °C,
Time 252000 sec
69 %
@Temperature 302 °F,
Time 70.0 hour
Plied; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 162 °C
@Time 1800 sec
324 °F
@Time 0.500 hour
Cure
 
Descriptive Properties
ColorOff white
Compound NumberA40-03
FormSheetUncompounded Viton
Formulation as Tested100VTR-9217
 30MT Black
 6Ca(OH)2
OdorNoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® ETP-900 Fluoroelastomer (FKM)
Chemours Viton® A-601C with 15 MT Black Fluoroelastomer Compound
Chemours Viton® A-601C Fluoroelastomer Compound
Chemours Viton® A-500 Fluoroelastomer Compound
Chemours Viton® A-401C Fluoroelastomer Compound

PDVC9946 / 170587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.