MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Carbon Fiber Filled; Polycarbonate (PC)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.40 g/cc0.0423 - 0.0506 lb/in³Average value: 1.28 g/cc Grade Count:31
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 21.6 % Grade Count:8
Water Absorption 0.100 %0.100 %Average value: 0.100 % Grade Count:7
Additive Loading 10.0 - 40.0 %10.0 - 40.0 %Average value: 26.3 % Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.0250 cm/cm0.000500 - 0.0250 in/inAverage value: 0.00217 cm/cm Grade Count:19
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 67.6 - 165 MPa9800 - 24000 psiAverage value: 106 MPa Grade Count:33
Elongation at Break 0.500 - 4.00 %0.500 - 4.00 %Average value: 1.67 % Grade Count:31
Modulus of Elasticity 4.61 - 16.5 GPa669 - 2400 ksiAverage value: 9.53 GPa Grade Count:33
Flexural Yield Strength 95.0 - 234 MPa13800 - 34000 psiAverage value: 151 MPa Grade Count:33
Flexural Modulus 3.51 - 17.9 GPa509 - 2600 ksiAverage value: 9.04 GPa Grade Count:33
Izod Impact, Notched 0.374 - 1.20 J/cm0.700 - 2.25 ft-lb/inAverage value: 0.767 J/cm Grade Count:31
Izod Impact, Unnotched 1.76 - 5.34 J/cm3.30 - 10.0 ft-lb/inAverage value: 3.32 J/cm Grade Count:31
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00 - 1.00e+9 ohm-cm1.00 - 1.00e+9 ohm-cmAverage value: 6.67e+7 ohm-cm Grade Count:20
Surface Resistance 0.0300 - 1.00e+12 ohm0.0300 - 1.00e+12 ohmAverage value: 2.89e+10 ohm Grade Count:23
Static Decay 0.500 - 2.00 sec0.500 - 2.00 secAverage value: 1.00 sec Grade Count:12
Shielding Effectiveness 25.0 - 60.0 dB25.0 - 60.0 dBAverage value: 46.0 dB Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 - 50.0 µm/m-°C7.22 - 27.8 µin/in-°FAverage value: 25.4 µm/m-°C Grade Count:9
Thermal Conductivity 0.560 - 0.700 W/m-K3.89 - 4.86 BTU-in/hr-ft²-°FAverage value: 0.617 W/m-K Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 97.2 - 118 °C207 - 245 °FAverage value: 105 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 93.9 - 129 °C201 - 265 °FAverage value: 113 °C Grade Count:20
UL RTI, Mechanical without Impact 70.0 - 105 °C158 - 221 °FAverage value: 86.7 °C Grade Count:9
Flammability, UL94 HB - V-0HB - V-0Grade Count:22
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 - 266 °C450 - 510 °FAverage value: 249 °C Grade Count:8
Nozzle Temperature 243 - 277 °C469 - 531 °FAverage value: 263 °C Grade Count:11
Melt Temperature 221 - 277 °C430 - 531 °FAverage value: 260 °C Grade Count:23
Mold Temperature 41.0 - 93.3 °C106 - 200 °FAverage value: 64.6 °C Grade Count:31
Drying Temperature 82.2 - 93.3 °C180 - 200 °FAverage value: 92.1 °C Grade Count:14
Moisture Content 0.0200 - 2.00 %0.0200 - 2.00 %Average value: 0.187 % Grade Count:25
Dew Point -28.9 °C-20.0 °FAverage value: -28.9 °C Grade Count:12
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Overview of materials for PC/ABS + Stainless Steel
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled

O1172a / 89062

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.