MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0045 cm/cm0.0020 - 0.0045 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0075 cm/cm0.0050 - 0.0075 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  130 MPa
@Temperature 150 °C
18900 psi
@Temperature 302 °F
 150 MPa
@Temperature 120 °C
21800 psi
@Temperature 248 °F
 175 MPa
@Temperature 90.0 °C
25400 psi
@Temperature 194 °F
 190 MPa
@Temperature 60.0 °C
27600 psi
@Temperature 140 °F
 205 MPa
@Temperature 23.0 °C
29700 psi
@Temperature 73.4 °F
Elongation at Break  1.9 %
@Temperature 23.0 °C
1.9 %
@Temperature 73.4 °F
 1.9 %
@Temperature 60.0 °C
1.9 %
@Temperature 140 °F
 2.0 %
@Temperature 90.0 °C
2.0 %
@Temperature 194 °F
 2.0 %
@Temperature 120 °C
2.0 %
@Temperature 248 °F
 2.0 %
@Temperature 150 °C
2.0 %
@Temperature 302 °F
Tensile Modulus  12.8 GPa
@Temperature 150 °C
1860 ksi
@Temperature 302 °F
 13.0 GPa
@Temperature 120 °C
1890 ksi
@Temperature 248 °F
 13.7 GPa
@Temperature 90.0 °C
1990 ksi
@Temperature 194 °F
 13.9 GPa
@Temperature 60.0 °C
2020 ksi
@Temperature 140 °F
 14.2 GPa
@Temperature 23.0 °C
2060 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 230 °C446 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C>= 572 °F
Deflection Temperature at 1.8 MPa (264 psi) 295 °C563 °F
Vicat Softening Point >= 300 °C
@Load 5.00 kg
>= 572 °F
@Load 11.0 lb
Flammability, UL94  V-1
@Thickness 0.750 mm
V-1
@Thickness 0.0295 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Glow Wire Test 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature 875 °C
@Thickness 1.00 mm
1610 °F
@Thickness 0.0394 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 370 - 400 °C698 - 752 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 120 - 150 °C
@Time 10800 sec
248 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akrotek® PEEK GF 40 natural (5068) PEEK, Dry, 40% Glass Filled
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled

PLATH9637 / 177333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.