MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cadi 1815 Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Zirconium addition to chromium copper improves creep resistance at high operating temperatures and reportedly reduces sticking of electrodes to the work during spot welding of galvanized materials. C18150 is specified mainly for electrode application.

Forms:

  • Rod
  • Bar
  • Plate

Information provided by Cadi Company.

Key Words: UNS C18150
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  65
@Diameter 50.8 - 76.2 mm
65
@Diameter 2.00 - 3.00 in
 70
@Diameter 25.4 - 50.8 mm
70
@Diameter 1.00 - 2.00 in
 >= 75
@Diameter <=25.4 mm
>= 75
@Diameter <=1.00 in
heat treated
Tensile Strength at Break >= 379 MPa>= 55000 psiAny thickness
Tensile Strength, Yield >= 379 MPa
@Strain 0.5 %
>= 55000 psi
@Strain 0.5 %
Any thickness
Modulus of Elasticity 117 GPa17000 ksi
Poissons Ratio 0.1810.181
Shear Modulus 49.6 GPa7200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000382 ohm-cm<= 0.00000382 ohm-cm>75 %IACS, up to 3" diameter/any thickness
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 323.4 W/m-K2244 BTU-in/hr-ft²-°F
Melting Point 980.0 - 1080 °C1796 - 1976 °F
Solidus 980.0 °C1796 °F
Liquidus 1080 °C1976 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 649 °C1200 °FBrazing, <15 minutes
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 1.0 %1.0 %
Copper, Cu 98.85 %98.85 %
Zirconium, Zr 0.15 %0.15 %
 
Descriptive Properties
RMWA Class2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 50 - 120 mm.
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 10 - 25 mm.
UNS C81500, Copper Casting Alloy
Copper, UNS C18100, Cold Worked (90% reduction) Wire, aged

NCADI11 / 15519

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.