MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock 8798 Neoprene Rubber Diaphragm, Nylon Insert
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Neoprene rubber with 13oz. nylon fabric insert

Combines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any service condition

Information provided by Garlock Rubber Technologies

Key Words: chloroprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65 - 7565 - 75
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 5.04 kV/mm
@Thickness 3.17 mm
128 kV/in
@Thickness 0.125 in
Unconditioned; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Monarch® F-02001 Neoprene Based Rubber Foam
Garlock 244 Neoprene Rubber - Commercial Grade
Garlock 5260 Neoprene Sheet Rubber
Polychloroprene Rubber (CR)
DuPont Mobility and Materials Neoprene FB Polychloroprene Rubber

PGARL852 / 157540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.