MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RSP Technology RSA-444 T6 Aluminum Super Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Used for Micro Engines. RSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling rates can be reached, converting more than 1 million degrees per second. As a result very fine nanostructured alloys with new functionalities are being developed and produced.

Information provided by RSP Technology BV

Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.63 g/cc0.0950 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200
Tensile Strength, Ultimate 465 MPa67400 psi
 160 MPa
@Temperature 300 °C,
Time 1800 sec
23200 psi
@Temperature 572 °F,
Time 0.500 hour
 260 MPa
@Temperature 250 °C,
Time 1800 sec
37700 psi
@Temperature 482 °F,
Time 0.500 hour
 360 MPa
@Temperature 200 °C,
Time 1800 sec
52200 psi
@Temperature 392 °F,
Time 0.500 hour
 410 MPa
@Temperature 150 °C,
Time 1800 sec
59500 psi
@Temperature 302 °F,
Time 0.500 hour
 430 MPa
@Temperature 100 °C,
Time 1800 sec
62400 psi
@Temperature 212 °F,
Time 0.500 hour
Elongation at Break 2.0 %
@Temperature 250 °C
2.0 %
@Temperature 482 °F
Tensile Modulus 96.0 GPa13900 ksi
Fatigue Strength 105 MPa
@Temperature 250 °C
15200 psi
@Temperature 482 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.6 µm/m-°C8.11 µin/in-°F
Thermal Conductivity 115 W/m-K798 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 62.9 %62.9 %
Copper, Cu 1.5 %1.5 %
Iron, Fe 2.7 %2.7 %
Magnesium, Mg 1.2 %1.2 %
Nickel, Ni 2.7 %2.7 %
Silicon, Si 30 %30 %
 
Descriptive Properties
Specific Stiffness37GPa/(g/cc)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RSP Technology RSA-462 T6 Aluminum Super Alloy
RSP Technology RSA-441 T6 Aluminum Super Alloy
RSP Technology RSA-443 AE Aluminum Super Alloy
RSP Technology RSA-483 AH Aluminum Super Alloy
RSP Technology RSA-453 AH Aluminum Super Alloy

NRSP44 / 160447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.