MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

I. Stern IS-84 Polyethylene Terephthalate Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: IS-84 is bottle grade PET resin manufactured using DuPont’s technology. It is typically used for carbonated drinks, agricultural chemicals, and APET sheet and PET strapping. IS-84 is engineered to provide good processability, excellent clarity/gloss, and very good mechanical properties. IS-84 resin is considered safe for food-packaging applications based on compliance with FDA regulation 21 CFR Section 177.1630 & other similar food contact safety regulations, manufactured as per ISO 22000 certified system (FSMS).

Information provided by I. Stern & Co. Inc.

I. Stern & Co. Inc. has been acquired by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Test 82 - 86 cm³/g0.82 - 0.86 dl/gIntrinsic Viscosity; ASTM D4603-03
Crystallinity >= 50 %>= 50 %QAF-PCL-3.415
 
Chemical PropertiesMetricEnglishComments
Acetaldehyde <= 1.0 ppm<= 1.0 ppmQAF - PCL
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Chips67 chips per gramQAF-PCL
Color "b"-3 to 0Hunterlab / QAF-PCL-3.211
Color "L"84 to 86Hunterlab / QAF-PCL-3.211
Fines<100 ppmSieve Shaker QAF-PCL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SABIC BC 110 Crystalline Polyethylene Terephthalate
Eastman BD445 PET
Dow LIGHTER™ C98 Polyethylene Terephthalate (PET) Resin
DuPont Mobility and Materials Rynite® FR530L NC010 Polyethylene Terephthalate (PET)
Versalis Eraclene® ML 70 U High Density Polyethylene - Injection Molding

PISTER931 / 192617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.