MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Features

PBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending, tensial strength, toughness. Does not absorb water, that means that identical properties are maintained also in wet environment. Melt is characterised by very good rheology, which enables manufacturing of extremely multiple products with complicated downflow-path. Anisotropy of shrinkage is much better in comparison with PA, what influences the manufacturing of round, cylindric or other hole products. Application in the automotive, electrical and engineering industry - connectors of cable harnesses, car-door locks, connection links, grips etc. Delivered in natural mode and in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³
Linear Mold Shrinkage 0.0091 cm/cm0.0091 in/in
Linear Mold Shrinkage, Transverse 0.0109 cm/cm0.0109 in/in
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 270 °C
10 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi
Elongation at Break 2.1 %2.1 %
Tensile Modulus 9.80 GPa1420 ksi
Flexural Strength 180 MPa26100 psi
Flexural Modulus 8.20 GPa1190 ksi
Charpy Impact Unnotched  4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
 4.80 J/cm²
@Temperature -20.0 °C
22.8 ft-lb/in²
@Temperature -4.00 °F
Charpy Impact, Notched  0.650 J/cm²
@Temperature -20.0 °C
3.09 ft-lb/in²
@Temperature -4.00 °F
 0.670 J/cm²
@Temperature 23.0 °C
3.19 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 - 225 °C433 - 437 °F
Deflection Temperature at 1.8 MPa (264 psi) 177 °C351 °F
Vicat Softening Point 178 °C352 °FB
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 50.0 - 90.0 °C122 - 194 °F
Drying Temperature 120 °C248 °F
Dry Time 4 hour4 hour
Moisture Content 0.050 %0.050 %
Injection Pressure 60.0 - 100 MPa8700 - 14500 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BLUESTAR 101G30 PBT, 30% Glass Filled
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre
Covestro Bayfill® EA 6005 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Celanese Celanex® 2000-2 PBT, Unfilled

PPLACO207 / 120831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.