MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Monmouth Rubber & Plastics Durafoam™ PMR 150 EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Performance Features:
  • Softness, stiffness & density infinitely variable.
  • High Ozone Resistance.
  • High Ultraviolet Resistance.
  • Non-Staining.
  • Made from Heat Resistant EPDM
  • Non-fogging (plasticizer free).
  • Dimensionally Stable (Very Low Shrinkage).
  • Unique Soft, Supple, Real Rubber Feel.
  • Very Fine Cell Structure.
  • Thermoformable – deep draw potential
  • Can be heat and flame laminated.
  • Butt-weldable – Both heat and/or adhesive
  • Bonds well to most pressure sensitive adhesives including economy rubber based adhesives.
  • Available standard in black.
  • Available on special order in custom bright colors.

Information provided by Monmouth Rubber & Plastics Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0641 g/cc0.00231 lb/in³ASTM D3575
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.0345 - 0.0621 MPa5.00 - 9.00 psiDeflection @ 25%; ASTM D1056-00
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber
Eurofoam Porocell POR 300/60 Ethylene Octane Metallocene EPDM Foam
Garlock 563 EPDM Sheet Rubber
Trelleborg E450 EPDM Rubber

PMONM015 / 160817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.