MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik BREAK-THRU® S 240 Surfactants
Categories: Fluid

Material Notes: Product description: BREAK-THRU® S 240 is a polyether trisiloxane. In aqueous solutions, it gives super spreading and does dramatically reduce surface tension. Therefore, the biological performance of crop protection products can be significantly enhanced by
  • superior wetting of hydrophobic surfaces, in particular leaves and other parts of plants,
  • better uptake through penetration of cuticular waxes, and
  • stomatal flooding.
Application: BREAK-THRU® S 240 can be used in tank mix applications as well in formulations. Please inquire for details. For tank-mixtures, pesticide manufacturers may suggest a rate of a non-ionic surfactant to be used with their product. Follow the corresponding label recommendation. However, if the pesticide label does not have a specific recommendation for adjuvant use, but does not prohibit its application, BREAK-THRU® S 240 should be applied at rates listed here. Further experimental work may be required to identify the specific dose rate of BREAK THRU® S 240 when it is incorporated into a specific pesticide formulation. Careful observation of spray performance in a trial application with the tank mixture to be sprayed is advised to determine proper and efficient rates.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Viscosity 40 - 90 cP40 - 90 cP
Surface Tension 22 dynes/cm22 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -10.0 °C<= 14.0 °F
Flash Point >= 100 °C>= 212 °F
 
Descriptive Properties
AppearanceColorless to pale straw liquid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5878 Additive
Aremco Quartz-Coat™ 845-D / 845-S High Temperature Specialty Coatings Inorganic, Silicon Filled
Titanium Aluminum Nitride (TiAlN) PVD Coating
Evonik BREAK-THRU® ADVANCE Surfactants
Evonik BREAK-THRU® Vibrant Surfactants

PEVONIL707 / 196911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.