MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® DX9303 Nylon 612  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: High-viscosity, plasticized, heat- and light-stabilized, impact-modified polyamide 612 compound for extrusion. VESTAMID DX9303 is a PA 612 extrusion compound developed for the production of tubing systems with higher requirements for heat resistance. The melting point of VESTAMID DX9303 is about 35°C higher than PA 11 and PA 12 compounds, allows higher peak temperatures in use. Thereby this compound fulfills the increased demands resulting from higher temperatures in the engine compartment. If it is intended to use VESTAMID DX9303 for fuel lines, certain preconditions must be observed. At temperatures above 100°C tubing of VESTAMID DX9303 allow a higher pressure load than tubing made of PA 12 compounds with comparable flexibility. The material absorbs only little moisture. Therefore dimensions and properties of parts are nearly unaffected through ambient conditions.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.027 cm/cm0.027 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 275 °C
11 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 38.0 MPa5510 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
Elongation at Yield 26 %26 %ISO 527
Tensile Modulus 0.900 GPa131 ksiISO 527
50% Modulus 37.0 MPa
@Strain 50 %
37.0 MPa
@Strain 50 %
ISO 527
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 8.70 J/cm²
@Temperature 23.0 °C
41.4 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C
@Temperature 23.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 211 °C412 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C68.0 °FISO 11357-1/-2
Flammability Test  1.0
@Thickness 1.60 mm
1.0
@Thickness 0.0630 in
IEC 60695-11-10
 1.0
@Thickness 3.20 mm
1.0
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Mold Temperature 80.0 °C176 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® X7293 Nylon 12, Extrusion/Tubing Grade
Evonik Vestamid® L2124 Plasticized Nylon 12
Evonik VESTAMID® E62-S1 Nylon 12 Elastomer
Evonik VESTAMID® Care ML94 Medical Grade Nylon 12
Evonik VESTAMID® Care ME71 Medical Grade Nylon 12

PEVONIK828 / 243037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.