MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ASTM A573 Steel, grade 65
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Carbon-manganese-silicon steel plate, structural quality
Improved toughness

Intended for fusion welding and for service at atmospheric temperatures where improved notch toughness is important. Mn content is exceedable if C content plus Mn content is < 0.40%. The following are suggested consumables for arc welding processes: Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E7015, E7016, E7018, E7028; Submerged Arc (AWS A5.23) F7x-Exxx; Gas Metal-Arc (AWS A5.28) ER70S-x; Flux Cored-Arc (AWS A5.29) E7xT-x except -2, -3, -10, or -GS.

Similar entries in MatWeb include: ASTM A573 grade 50, grade 70

Key Words: UNS K02404
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/inĀ³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 450 - 530 MPa65300 - 76900 psi
Tensile Strength, Yield 240 MPa34800 psi
Elongation at Break 20 %20 %in 200 mm
Bulk Modulus 160 GPa23200 ksiTypical for steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.26 %0.26 %may vary with plate thickness
Iron, Fe 98 %98 %as balance
Manganese, Mn 0.85 - 1.2 %0.85 - 1.2 %
Phosphorus, P 0.040 %0.040 %
Silicon, Si 0.15 - 0.40 %0.15 - 0.40 %
Sulfur, S 0.050 %0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A573 Steel, grade 58
ASTM A573 Steel, grade 70
ASTM A284 Steel, grade C
ASTM A284 Steel, grade D
ASTM A537 Carbon Steel, Class 2

MS573B / 13990

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.