MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hanwha Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural thin wall applications and where good glass distributions into features such as ribs and bosses is desired.

Mechanical properties and mold shrinkage measured on flat plaques.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccLaminate; ISO 1183
 1.15 g/cc1.15 g/ccMolded; ISO 1183
Filler Content 31 %31 %By weight (ashing); Internal
Thickness 4320 microns170 milSheet; Internal
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inMeasured on flat plaques; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psiISO 527
Elongation at Break 2.8 %2.8 %ISO 527
Tensile Modulus 4.528 GPa656.7 ksiISO 527
Flexural Strength 97.7 MPa14200 psiISO 178
Flexural Modulus 4.26 GPa618 ksiISO 178
Poissons Ratio 0.4280.428ISO 527
Izod Impact, Notched (ISO) 27.9 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
13.3 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Impact 2629
@Thickness 102 mm
2629
@Thickness 4.00 in
N; Multi-axial, at max. load; ASTM D3763
Impact Test  12.1 J
@Thickness 102 mm
8.92 ft-lb
@Thickness 4.00 in
Multi-axial, at max. load; ASTM D3763
 21.4 J
@Thickness 102 mm
15.8 ft-lb
@Thickness 4.00 in
Multi-axial, at failure; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 51.2 µm/m-°C
@Temperature -40.0 - 120 °C
28.4 µin/in-°F
@Temperature -40.0 - 248 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75
 
Descriptive Properties
ColorBlackInternal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hanwha Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C401-B01 40% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
Hanwha Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix

PZZGEAZ62 / 40611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.