MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cadmium Copper, UNS C16200, Drawn (>99%) Temper wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability.

Applications: trolley wire, heating pads, electric-blanket elements, spring contacts, railbands, high-strength transmission lines, connectors, cable wrap, switch gear components and wave guide cavities.

Test specimen: wire - 0.25mm diameter; drawn(>99%) temper.

Key Words: C108, ISO CuCd1, A1/3, cadmium bronze, copper-cadmium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 690 MPa100000 psi
Elongation at Break 1.0 %1.0 %in 1.5 m
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000192 ohm-cm
@Temperature 20.0 °C
0.00000192 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 360 W/m-K2500 BTU-in/hr-ft²-°F
Melting Point 1030 - 1076 °C1890 - 1969 °F
Solidus 1030 °C1890 °F
Liquidus 1076 °C1969 °F
Annealing Point 427 - 760 °C800 - 1400 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 750 °C797 - 1380 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 0.70 - 1.2 %0.70 - 1.2 %
Copper, Cu 98.78 - 99.3 %98.78 - 99.3 %
Iron, Fe <= 0.020 %<= 0.020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oilite® Bronze Bearing Alloy - SAE 841
AISI 1018 Steel, cold drawn
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Chromium Copper, UNS C18200, TB00 Temper flat products
Cadmium-Copper, Deoxidized, UNS C14310

MC16200c4 / 10717

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.