MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KEP Kepital® F20-52G Acetal Copolymer, Low Gloss UV & Weather Resistance Grade
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Low gloss, UV resistance, easy-flow grade for general injection molding. F20-52G is suited for parts requiring a good weather resistance and low gloss characteristic.

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 58.0 MPa8410 psi50 mm/min; ISO 527
Elongation at Break 40 %40 %50 mm/min; ISO 527
Elongation at Yield 11 %11 %50 mm/min; ISO 527
Flexural Strength 78.0 MPa11300 psiISO 178
Flexural Modulus 2.35 GPa341 ksiISO 178
Charpy Impact, Notched 0.710 J/cm²3.38 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Strength 19.0 kV/mm483 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 13021 POM, Unfilled
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
KEP Kepital® MX25BT01 Acetal Copolymer, Medical Grade
KEP Kepital® MX20BT01 Acetal Copolymer, Medical Grade
KEP Kepital® FL2010 Acetal Copolymer, PTFE modified

PKEP9935 / 185611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.