MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type 304HN Stainless Steel, Annealed Bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: High Nitrogen 304 stainless steel. Austenitic Cr-Ni stainless steel. Nitrogen provides higher tensile and tensile yield strength without diminishing ductility, corrosion resistance, or nonmagnetic properties. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion.

Applications: Aircraft and Aerospace components, marine components, high temperature components, pressure vessels, pump components, welded tubing, forged fittings, pipe flanges, and valves.

Weldability: Can be brazed and welded using common methods. Grain-boundary carbide precipitation can occur in heat-affected zones (HAZ). Annealing will restore corrosion resistance to the weldment.

Key Words: aisi304, AISI 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, T304HN, 304HN, 304 HN, UNS S30452, ASTM A 276 A276
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 620 MPa89900 psi
Tensile Strength, Yield 345 MPa50000 psi
Elongation at Break 30 %30 %
Reduction of Area 50 %50 %
Modulus of Elasticity 197 GPa28600 ksiestimated from comparison of similar stainless steels.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm
@Temperature 20.0 °C
0.0000720 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.9 µm/m-°C
@Temperature 0.000 - 650 °C
10.5 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 66 - 73.8 %66 - 73.8 %as balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 10.5 %8.0 - 10.5 %
Nitrogen, N 0.16 - 0.30 %0.16 - 0.30 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 304HN Stainless Steel
304 Stainless Steel
AISI Type 304L Stainless Steel
304 Stainless Steel (UNS S30400); Annealed Bar
AISI Type 304N Stainless Steel

MQ304HNb / 171839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.