MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram RamOfin PPC301G2 Polypropylene, 10% Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: 10% glass fibers reinforced polypropylene copolymer for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³DIN 53479
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM-D785
Tensile Strength, Yield 35.0 MPa5080 psiASTM-D638
Elongation at Break 3.0 %3.0 %ASTM-D638
Flexural Strength 50.0 MPa7250 psiASTM D790
Flexural Modulus 1.20 GPa174 ksiASTM-D790
Izod Impact, Notched 1.70 J/cm
@Temperature 23.0 °C
3.18 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °F
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Higlass SB224-1 Polypropylene Copolymer, 10% Glass Fiber
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Entec Hypro™ F PPC-GF10 Natural Impact Polypropylene, 10% Glass Reinforced
Cheng Yu Plastic PP236G1 Polypropylene, 10% Glass Fiber
Chem Polymer Formax 605 G Acetal, 5% Glass Reinforced

PPOLYRA313 / 57575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.