MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® C513UV HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Resin Type: Hexene Copolymer

Characteristics:

  • Outstanding impact resistance
  • Excellent ESCR
  • Excellent processability
  • UV stabilization

Applications:

  • Intermediate bulk containers
  • Agricultural containers

Information provided by Chevron Phillips.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D1505
ESCR 100% Igepal® >= 2000 hour>= 2000 hourConditions A and B; ASTM D1693
Melt Flow 6.2 g/10 min6.2 g/10 minCondition 190/2.16, HLMI; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength, Yield 24.0 MPa3480 psi2 in/min, Type IV bar; ASTM D638
Elongation at Break 700 %700 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.07 GPa155 ksiTangent, 16:1 span:depth,0.5in/min; ASTM D790
Tensile Impact Strength 580 kJ/m²276 ft-lb/in²Type S bar; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C151 °FMethod A; ASTM D648
Vicat Softening Point 123 °C253 °FLoading 1, Rate A; ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FType A, type 1 specimen; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® FB3450 HDPE for Film Extrusion
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Equate EMDA-6147 HDPE Blow Molding Resin
Formosa Plastics Formolene® HB5502Z Blow Molding HDPE
Global B-5200 High Density Polyethylene

PCHEVD016 / 20634

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.