MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ferro Zirmonite 200, ZTA
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: ZTA, ZrO2, zirconia, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.48 g/cc0.162 lb/in³
Water Absorption 0.00 %0.00 %
Open Porosity 0.00 %0.00 %Gas tight. Test with helium mass spectrometer
Weibull Modulus 1111
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 15001500KHN5 microhardness, kg/mm²
Vickers Microhardness 16501650HV5 microhardness, kg/mm²
Tensile Strength, Ultimate 481 MPa69800 psiACMA Test #4
Modulus of Elasticity 278 GPa40300 ksiultrasonic
Compressive Strength 2930 MPa425000 psiASTM C773-74
Poissons Ratio 0.220.22ASTM C623
Fracture Toughness 6.50 MPa-m½5.92 ksi-in½Kic (indentation)
Shear Modulus 114 GPa16500 ksiultrasonic
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.80 µm/m-°C
@Temperature 25.0 - 200 °C
4.33 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM C32
 8.50 µm/m-°C
@Temperature 25.0 - 500 °C
4.72 µin/in-°F
@Temperature 77.0 - 932 °F
ASTM C32
 9.10 µm/m-°C
@Temperature 25.0 - 800 °C
5.06 µin/in-°F
@Temperature 77.0 - 1470 °F
 9.10 µm/m-°C
@Temperature 25.0 - 1000 °C
5.06 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C32
Thermal Conductivity 15.8 W/m-K110 BTU-in/hr-ft²-°F
 6.40 W/m-K
@Temperature 1000 °C
44.4 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 7.50 W/m-K
@Temperature 800 °C
52.0 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 12.1 W/m-K
@Temperature 400 °C
84.0 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5052-H32
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), as-rolled
AISI Type 304HN Stainless Steel
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2

CFC013 / 811

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.