Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications. Dexflex 1066-UV YGYA is a thermoplastic olefin elastomeric (TPO) typically used for automotive exterior applications that require durable paintability in large injection molded parts. Applications: Exterior Automotive Applications Information provided by LyondellBasell. |