MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Trinseo Plexiglas® SG7 Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Gamma Radiation Resistant, Molded

Material Notes: Plexiglas® SG7 is an impact-modified acrylic resin suitable for injection molding and extrusion. It is a high flow resin designed to provide outstanding light transmission and water white clarity for disposable medical applications.

Some of the features and benefits of Plexiglas® SG7 are

  • Chemical Resistance: Good resistance to lipids and drug formulations, Good resistance to isopropyl alcohol (IPA), Property retention after exposure to hospital antiseptics, acids and bases
  • Sterilization: Stable to gamma radiation, E-beam, and ETO, Rapid recovery with excellent color stability, Retention of transparency and clarity, Retention of mechanical properties
  • Durability and Processability: Moldflow simulation data available, Excellent melt processability, Reduced cycle times, Suitable for thin-wall applications and complex multi-cavity molds, Good bondability using solvent, ultrasonic, or radio frequency methods
Appearance: Clear/Transparent

Characteristics: Alcohol Resistant; Biocompatible; Bondability; BPA Free; Chemical Resistant; High Clarity; ESCR, High (Stress Crack Resist.); High Impact Resistance; Good Moldability; Radiation (Gamma) Resistant; Sterilization, E-beam; Sterilization, Ethylene Oxide

Applications: Medical/Healthcare Applications; Medical Appliances

Agency Ratings: ISO 10993-4; ISO 10993-5; USP CLASS VI

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Water Absorption 0.30 %0.30 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 10 g/10 min
@Load 3.80 kg,
Temperature 230 °C
10 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060ASTM D785
Tensile Strength, Ultimate 46.9 MPa6800 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Tensile Modulus 2.45 GPa355 ksiASTM D638
Flexural Strength <= 85.5 MPa<= 12400 psiASTM D790
Flexural Modulus 2.45 GPa355 ksiASTM D790
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.202 W/m-K1.40 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C190 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.7 °C179 °Fannealed; ASTM D648
Vicat Softening Point 83.3 °C182 °F50°C/hr; 50N; ASTM D1525
 93.9 °C201 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49
@Temperature 22.8 °C
1.49
@Temperature 73.0 °F
ND; ASTM D542
Haze <= 2.0 %
@Thickness 3.17 mm
<= 2.0 %
@Thickness 0.125 in
ASTM D1003
Transmission, Visible 91 %
@Thickness 3.17 mm
91 %
@Thickness 0.125 in
ASTM D1003
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® MI7 Acrylic
Trinseo Plexiglas® V920 Acrylic
Trinseo Plexiglas® DR® Acrylic
Trinseo Plexiglas® V052 Acrylic
Trinseo Solarkote™ A200 Acrylic

PARKG041 / 24395

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.