MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6.

High-Strength, Intermediate Temperature Alloy

Features: TIMETAL 6-2-4-6 is a stronger derivative of TIMETAL 6-2-4-2 offering higher strength, depth hardenability and elevated temperature properties up to 450°C. This alloy is similar in forgeability and crack sensitivity to TIMETAL 6-4. This alloy is used in intermediate compressor stages of turbine engines for disks and blades, seals, and for airframe parts. It is nonmagnetic.

Data provided by TIMET.

Key Words: UNS R56260
Vendors:
TITANIUM ENGINEERS is your source for high strength, NACE titanium alloys, with a full range of stock sizes and sizes made to order. Our in-house metallurgical experts ensure the best alloy selection and process titanium to meet unique customer specifications. Please visit our website www.TitaniumEngineers.com for more information or call us at +1 281 265 2910 (USA) or +44 (0) 1675 464200 (UK).

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.64 g/cc0.168 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1240 MPa180000 psi
Tensile Strength, Yield 1151 MPa166900 psi
Elongation at Break 14 %14 %
Reduction of Area 42 %42 %
Modulus of Elasticity 115 GPa16700 ksiTypical
 100 GPa
@Temperature 425 °C
14500 ksi
@Temperature 797 °F
 107 GPa
@Temperature 315 °C
15500 ksi
@Temperature 599 °F
Fatigue Strength  276 MPa
@# of Cycles 1.00e+7
40000 psi
@# of Cycles 1.00e+7
notched
 675 MPa
@# of Cycles 1.00e+7
97900 psi
@# of Cycles 1.00e+7
smooth
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000190 - 0.000205 ohm-cm0.000190 - 0.000205 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 100 °C
5.00 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.502 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 7.61 W/m-K52.8 BTU-in/hr-ft²-°F
Melting Point 1595 - 1675 °C2903 - 3047 °F
Solidus 1595 °C2903 °F
Liquidus 1675 °C3047 °F
Beta Transus 940 °C1720 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.5 %5.5 - 6.5 %
Carbon, C <= 0.040 %<= 0.040 %
Hydrogen, H <= 0.125 %<= 0.125 %
Iron, Fe <= 0.15 %<= 0.15 %
Molybdenum, Mo 5.5 - 6.5 %5.5 - 6.5 %
Nitrogen, N <= 0.040 %<= 0.040 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.15 %<= 0.15 %
Tin, Sn 1.75 - 2.25 %1.75 - 2.25 %
Titanium, Ti 79.4 - 83.7 %79.4 - 83.7 %Calculated as remainder
Zirconium, Zr 3.6 - 4.4 %3.6 - 4.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical

NTIME6246D / 19312

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.